nebula storm cement
LAB SAMPLE:
Fillers: 54.2%
Stones: 30.3%
Residues: 5.9%
(from construction demolition):from which: 100% concrete
Additives: 9.6%
LAB SAMPLE:
Fillers: 54.2%
Stones: 30.3%
Residues: 5.9%
(from construction demolition):from which: 100% concrete
Additives: 9.6%